5

Wearing Surface

(1/2″ Integral wearing surface) One large area of moderate scaling near the mid-span east half of the deck (180 SF). Some minor scaling at random locations (30 SF). Some pop-outs and insignificant cracking at random locations

5

Top of Deck

Some deep spalls (> 1″), mostly with exposed rebar near the mid-span of the deck (35 SF total)

8

Underside of Deck

Bay 1: SIP forms with isolated rust along the connection to the top flange of the girder. Bays 2 & 3: Reinforced concrete with no significant defects