From: Performance comparison of steel fiber reinforced concrete and conventional reinforced concrete cast-in-place half-scale concrete bridge decks under bending
Material
Weight Kg (lb)
Cement
403.2 (888.9)
Coarse Aggregate
739.1 (1629.4)
Fine Aggregate
1032.7 (2276.7)
Water
198.5 (437.6)
Total
2373.5 (5232.6)