Fig. 16From: Utilizing blast furnace ferronickel slag as paste replacement to reduce white Portland cement content and improve performance of mortarThe 28-day compressive strength of the PRB and CRB mortar samples versus the cement content of the mortar at W/C of 0.40 and 0.55Back to article page