Skip to main content

Table 3 Mix proportion of concrete

From: Development of a fast-hardening retarding high-early-strength concrete with low-alkalinity sulphoaluminate cement and practical application

Concrete

Water-cement ratio

Water (kg/m3)

Portland cement (kg/m3)

LASC (kg/m3)

Sand (kg/m3)

Rock (kg/m3)

Fly ash (kg/m3)

Mineral powder

(kg/m3)

Superplasticizer

(kg/m3)

Aluminum Sulfate (kg/m3)

Maximum diameter of the aggregate (mm)

C60

0.32

160

395

–

595

1105

55

50

10

–

25

FRHC

0.37

176

–

475

630

1165

–

 

7.125

6.05

15